bro.
if not mistaken, u r from miri rite??
may i know whr u get ur acylric??
project - acrylic casing!, page 1,3,6,8,9,10,12,13(NEW)!!
project - acrylic casing!, page 1,3,6,8,9,10,12,13(NEW)!!
|
|
Jun 9 2009, 01:12 PM
|
![]() ![]() ![]() ![]()
Senior Member
698 posts Joined: Mar 2008 From: Oil town @ Miri |
bro.
if not mistaken, u r from miri rite?? may i know whr u get ur acylric?? |
|
|
|
|
|
Jun 9 2009, 01:18 PM
|
![]() ![]() ![]() ![]()
Senior Member
507 posts Joined: Apr 2009 |
yea from miri XD
from my dad friend shop calling 益贸hardware shop ^^ i not sure the chinese how write but it is same sound |
|
|
Jun 9 2009, 01:54 PM
|
![]() ![]() ![]() ![]() ![]()
Senior Member
741 posts Joined: Feb 2008 |
QUOTE(2848calvin @ Jun 9 2009, 12:49 PM) on top ar...i thinking let the top and side panel clean clean 1 leh..XD but will think about tat ar and only 1 fan at the back outflow.. like that ar |
|
|
Jun 9 2009, 02:10 PM
|
![]() ![]() ![]() ![]() ![]() ![]()
Senior Member
1,140 posts Joined: May 2008 |
seriously... 3mm arcylic with extray support for the psu and mobo area is enuf
4mm is better... (can do it without support) anything over 4mm is just waste as it is very expensive... here is one of my old arcylic project » Click to show Spoiler - click again to hide... « This post has been edited by tjay_tj: Jun 9 2009, 02:34 PM |
|
|
Jun 9 2009, 02:12 PM
|
![]() ![]() ![]() ![]() ![]()
Senior Member
939 posts Joined: Jan 2007 |
» Click to show Spoiler - click again to hide... « may be u can try hot gun,make it left right few time to make it easy to bend. or just colorform to combine become L shape lo. i also thinkin wanna do a custom casing. |
|
|
Jun 9 2009, 02:37 PM
|
![]() ![]() ![]() ![]()
Senior Member
507 posts Joined: Apr 2009 |
QUOTE(karLz @ Jun 9 2009, 01:54 PM) so use 3 fan at the front and 1 at the back... how bout ur ventilation system... the front fan of course inflow rite... yea infront is intake and the one is blow maybe 2 fan at behind and only 1 fan at the back outflow.. like that ar Added on June 9, 2009, 2:38 pm QUOTE(tjay_tj @ Jun 9 2009, 02:10 PM) seriously... 3mm arcylic with extray support for the psu and mobo area is enuf hmm..4mm is enough ar?okok 4mm is better... (can do it without support) anything over 4mm is just waste as it is very expensive... here is one of my old arcylic project » Click to show Spoiler - click again to hide... « Added on June 9, 2009, 2:41 pm QUOTE(lun1986 @ Jun 9 2009, 02:12 PM) » Click to show Spoiler - click again to hide... « may be u can try hot gun,make it left right few time to make it easy to bend. or just colorform to combine become L shape lo. i also thinkin wanna do a custom casing. This post has been edited by 2848calvin: Jun 9 2009, 02:41 PM |
|
|
|
|
|
Jun 9 2009, 02:46 PM
|
![]() ![]() ![]() ![]() ![]()
Senior Member
801 posts Joined: Jan 2003 From: KBR-KUL-SIN |
wow bro...my dream lo want to build acrylic casing...put a blowhole on top la bro...exhaust on top...huhuhu..
so envy of u...if only i got enuf money to buy the acrylic..got lots of plans for a acrylic casing.. |
|
|
Jun 9 2009, 03:01 PM
|
![]() ![]() ![]() ![]()
Senior Member
507 posts Joined: Apr 2009 |
XD be4 holiday i save money thinking wan buy a 2nd hand casing and mod but miri no ppl sell =/ so use the money for buy acrylic lo ^^ mind to share ur plan with me?^^
|
|
|
Jun 9 2009, 03:58 PM
|
![]() ![]() ![]() ![]() ![]()
Senior Member
939 posts Joined: Jan 2007 |
hot gun is normal use to stick car tinted 1.
|
|
|
Jun 9 2009, 04:14 PM
|
![]() ![]() ![]() ![]()
Senior Member
507 posts Joined: Apr 2009 |
dun have tat hot gun
» Click to show Spoiler - click again to hide... « i make it damnn..i wanna start now...@@ waiting my dad pick me to the hardware shop =/ anyone can come and pick me?~~~ This post has been edited by 2848calvin: Jun 9 2009, 07:51 PM |
|
|
Jun 9 2009, 04:33 PM
|
![]() ![]() ![]() ![]() ![]()
Senior Member
939 posts Joined: Jan 2007 |
|
|
|
Jun 9 2009, 04:37 PM
|
![]() ![]() ![]() ![]()
Senior Member
507 posts Joined: Apr 2009 |
hvn buy yet @@.. i juz the heat heat thing to heat and bend the acrylic is so soft XD
|
|
|
Jun 9 2009, 04:52 PM
|
![]() ![]() ![]() ![]() ![]() ![]()
Senior Member
1,140 posts Joined: May 2008 |
that is 2mm arcylic rite?
haha btw, try using the iron to bend the arcylic... some ppl use boiling water |
|
|
|
|
|
Jun 9 2009, 05:02 PM
|
![]() ![]() ![]() ![]()
Senior Member
507 posts Joined: Apr 2009 |
tat is 3mm acrylic XD i stand inside my store juz now and think for so long using wat for heat then i saw tat thing hehe boiling water?o.o mmm....@@ the water ...i boiling a cup of water for u bro~~haha
|
|
|
Jun 9 2009, 05:11 PM
|
![]() ![]() ![]() ![]() ![]() ![]()
Senior Member
1,140 posts Joined: May 2008 |
QUOTE(2848calvin @ Jun 9 2009, 05:02 PM) tat is 3mm acrylic XD i stand inside my store juz now and think for so long using wat for heat then i saw tat thing hehe boiling water?o.o mmm....@@ the water ...i boiling a cup of water for u bro~~haha no thanks... i will be cold water after u sent it to kl... i can boil myself... |
|
|
Jun 9 2009, 07:22 PM
|
![]() ![]() ![]() ![]()
Senior Member
507 posts Joined: Apr 2009 |
XD i juz back~~~ juz order a arcylic panel i dontknow how big =/ my dad order it and i buy some screw,acrylic knife,glue stick,and 1 bottle 3 sec super glue ^^ cant wait till tmr~~~harharhar
|
|
|
Jun 9 2009, 08:00 PM
|
![]() ![]() ![]() ![]() ![]() ![]()
Senior Member
1,140 posts Joined: May 2008 |
just a advise... dun use super glue...
even the epoxy is useless... ask the shop u bought the arcylic for chloroform... more effective in gluing the arcylic. |
|
|
Jun 9 2009, 08:06 PM
|
![]() ![]() ![]() ![]()
Senior Member
507 posts Joined: Apr 2009 |
o.o really arr..okok tmr i go get it hehe the chloroform after use on acrylic the acrylic will become white white 1?
|
|
|
Jun 9 2009, 08:14 PM
|
![]() ![]() ![]() ![]() ![]() ![]()
Senior Member
1,140 posts Joined: May 2008 |
the problem is it wouldnt stick properly
it will break easily some superglue will not leave white thing after u apply... but i forget which already |
|
|
Jun 9 2009, 08:21 PM
|
![]() ![]() ![]() ![]()
Senior Member
507 posts Joined: Apr 2009 |
oh..hehe if whole casing use screw hmm...
|