tried the following on my Black Lexus IS250 with Optimum products.
Clay bar with MGs
LC Orange Pad with Optimum hyper compound on DA speed 6
LC White Pad with Optimum hyper polish on DA speed 4
MG W7006 wool pad with Optimum hyper compound on Rotary 1500RPM
LC White pad with Optimum hyper polish on DA speed 4
both setup did not yield any resulting in deminishing the micro swirls. I tried all pressured and non pressured way as i compound them, I still cant get any mirror finishing result.
I feel like going for MG 205
Anyone knows whats my issue here?>